Prouduct introduction:
TCHLEAD TD-20 applicable to purified cotton, polyester cotton and other fibers could increase modified starch and PVA adhesion of yarn, besides endow warp yarn with a good hairiness supple state. It can also increase the flexibility of serosa and improve the weaving ability of yarn. The result is particularly evident when it is used in purified cotton yarn. TECHLEAD TD-20 desizing easily and non-polluting has a good compatibility with the PVA, modified starch and other size, auxiliary agent.
Product Description:
ITEM: SPECIFICATIONS
Main Composition: Acrylate copolymer
Appearance(30℃): Colorless to yellowish transparent viscid liquid
Solid contents: 20±0.5%
PH: 6.0-7.5
Ionicity Anionic
Viscosity(4%,30℃,cps) 10~15
Package:
50L plastic drum
125L plastic drum
Storages:
The product must store in cool drying place,prtect from light,transport and store it keep up to 5℃,At least six months for good storage.